Abstract

A process for improving the continuity of overlayers above an aluminum metallization stripe on a semiconductor device which includes the step of forming a conversion coating on the surface of the aluminium metallization. The conversion coating has a higher etch rate than the aluminum per se, and hence after selective masking, a tapered or sloped edge is produced on the aluminum stripe which is more easily continuously overlayed by the further necessary layers.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 1 · Forward citations: 15.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    In a process for producing a semiconductor integrated circuit the steps comprising: (a) depositing an aluminum metallization layer over an insulating layer of a semiconductor substrate, (b) forming a conversion coating on the surface of the aluminum metallization layer by immersing the semiconductor substrate in fuming nitric acid and then subjecting the wafer to boiling water, (c) selectively masking said aluminum metallization layer, and (d) etching said aluminum metallization whereby said conversion coating etches more rapidly than the unconverted portion of the layer and forms a slop

  2. Claim 2Depends on #1

    In a process as recited in claim 1 wherein said fuming nitric acid is maintained at a temperature of approximately 80° C.

  3. Claim 3Independent Claim

    In a process for producing a semiconductor integrat

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 15 total)

PatentTitleYearCitations
US 7,294,578 B1Use of a plasma source to form a layer during the formation of a semiconductor device20070
US 6,525,404 B1Moisture corrosion inhibitor layer for Al-alloy metallization layers, particularly for electronic devices and corresponding manufacturing method20030
US 5,242,543 AWet etching method for forming metal film pattern having tapered edges199325
US 7,709,343 B2Use of a plasma source to form a layer during the formation of a semiconductor device20100
US 5,670,062 AMethod for producing tapered lines199747
US 6,762,123 B2Moisture corrosion inhibitor layer for Al-alloy metallization layers, particularly for electronic devices and corresponding manufacturing method20042
US 4,919,748 AMethod for tapered etching1990111
US 4,235,648 AMethod for immersion plating very thin films of aluminum198023
WO 8,500,928 A1Process for beveling a metal layer in an integrated circuit—3
US 4,351,698 AVariable sloped etching of thin film heads198211
US 2009017634 A1Use of a plasma source to form a layer during the formation of a semiconductor device—4
US 7,429,535 B2Use of a plasma source to form a layer during the formation of a semiconductor device20080
US 2003107109 A1Moisture corrosion inhibitor layer for Al-alloy metallization layers, particularly for electronic devices and corresponding manufacturing method—5
EP 1,101,837 A1Moisture corrosion inhibitor layer for Al-alloy metallization layers, particularly for electronic devices and corresponding manufacturing method—3
US 2007123048 A1Use of a plasma source to form a layer during the formation of a semiconductor device—0

References Cited — Backward Prior Art (1)