Process for manufacturing a gallium phosphide electroluminescent device
Abstract
When gallium phosphide is etched with hot phosphoric acid from the surface of a crystal having a (1 1 1) plane, the etched surface becomes a flat and smooth plane inclined at an angle of 45° to 55° to the (1 1 1) plane. Accordingly, when an electroluminescent diode is manufactured by forming a p-n junction on a gallium phosphide crystal having a (1 1 1) plane and etching the crystal with a hot concentrated phosphoric acid etching solution to form a mesa structure, the side faces of the resulting crystal becomes inclined to the plane of the junction at an angle of nearly 45° so that the visible rays generated in the p-n junction are totally reflected on the side faces, thus markedly increasing the intensity of emitted rays in the direction of the optical axis perpendicular to the principal plane of the p-n junction.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 20 · Forward citations: 29.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method for manufacturing a gallium phosphide electroluminescent device, characterized by providing an anticorrosive polygonal plane mask on the surface of a gallium phosphide crystal containing (1 1 1) planes, and etching the crystal from exposed areas with an aqueous solution consisting essentially of hot concentrated phosphoric acid to form a mesa structure in the form of a truncated polyhedral pyramid.
- Claim 2Depends on #1
A method according to claim 1, wherein the concentrated phosphoric acid solution contains 70% or more of phosphoric acid.
- Claim 3Depends on #1
A method according to claim 1, wherein the concentrated phosphoric acid solution is maintained at a temperature in the range of 130° to 220° C, preferably 150° to 180° C.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗