Process for making linear polyesters from ethylene glycol and terephthalic acid
Abstract
A batch process for esterifying ethylene glycol and terephthalic acid at elevated temperature and pressure in which a part of the ethylene glycol required for the complete esterification reaction is placed in an autoclave and heated under pressure, and the remainder of the glycol is added to said heated glycol in the form of a paste with terephthalic acid. Preferably the glycol initially present in the autoclave amounts to 0.3 to 0.8 moles per mole of terephthalic acid while the glycol added as a paste amounts to 1.4 to 0.9 moles per mole of terephthalic acid. The glycol initially in the autoclave may be glycol reclaimed from the mixture volatilized during the reaction and may contain up to 20% water, preferably 2-6% water.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 49.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A process for making linear polyesters by discontinuous direct esterification of ethylene glycol and terephthalic acid at molar ratios of 1.1:1 to 2.0:1, in which at the beginning of the esterification reaction heated glycol is placed in the reaction vessel and the terephthalic acid is fed into the glycol, followed by polycondensation of the esterification product, the improvement comprising: maintaining 0.1 to 1.4 moles of the glycol required for the esterification reaction per mole of the terephthalic acid at a temperature above 200° C at superatmospheric pressure in the said reaction vessel
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗