Epitaxial growth of bismuth rare earth iron garnet from a flux of bismuth oxide and alkali metal oxide

26Forward Citations (#2836623 Global)
0.5/yrCitation Velocity (#14689982 Global)
4.47Citation PageRank (#3975428 Global)
11Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method of growing a monocrystalline bismuth rare earth iron garnet material from a melt in which a flux containing bismuth oxide and an alkali metal oxide is employed.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 26.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    In the method of growing a monocrystalline bismuth rare earth iron garnet layer of the formula Bi p A 3-p D q Fe 5q O 12 wherein 0 < p < 3, 0 < q < 5, A is at least one rare earth selected from those elements having atomic numbers 21, 39 and 57 to 91 inclusive and D is at least one element selected from the group consisting of gallium and aluminum by liquid phase epitaxy from a melt on a crystal face of a monocrystalline substrate, the resulting layer having the crystallographic orientation of said crystal face, said melt comprising the components of said garnet and a flux, th

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 26 total)

PatentTitleYearCitations
US 5,277,845 AOxide garnet single crystal19945
US 2008095686 A1Magnetic Garnet Single Crystal and Optical Element Using Same as Well as Method of Producing Single Crystal—14
US 4,690,726 ALiquid phase epitaxial growth of bismuth-containing garnet films198712
US 4,544,438 ALiquid phase epitaxial growth of bismuth-containing garnet films19854
EP 1,820,886 A4Magnetic garnet single crystal, optical device using same and method for producing single crystal—0
US 5,322,591 AHydrothermal growth on non-linear optical crystals199413
US 2010326350 A1Magnetic garnet single crystal and optical element using same as well as method of producing single crystal—0
US 2007193504 A1Magnetic garnet single crystal and optical element using the same—12
US 4,582,562 AProcess for preparing a single oxide crystal19865
US 2007160875 A1Magnetic garnet single crystal and method for producing the same as well as optical element using the same—12
US 2006187546 A1Magnetic garnet material, faraday rotator, optical device, bismuth-substituted rare earth-iron-garnet single-crystal film and method for producing the same and crucible for producing the same—4
US 7,758,766 B2Magnetic garnet single crystal and Faraday rotator using the same20100
US 7,333,261 B2Magnetic garnet material, faraday rotator, optical device, bismuth-substituted rare earth-iron-garnet single-crystal film and method for producing the same crucible for producing the same200811
US 7,517,406 B2Magnetic garnet material, faraday rotator, optical device, bismuth-substituted rare earth-iron-garnet single-crystal film and method for producing the same and crucible for producing the same200911
US 6,368,401 B1Method of producing magnetic garnet single crystal film and magnetic garnet single crystal film having a nonuniform thickness20021

Non-Patent Literature (1)

  • Akselrad et al., AIP Conf. Proc., No. 18, prog. 2 (1973), pp. 949-953.