Patents
US 4,076,573 A#14695886 Most CitedExpiredUnited States (USPTO)Utility

Method of making planar silicon-on-sapphire composite

7Forward Citations (#14695886 Global)
0.1/yrCitation Velocity (#38327606 Global)
2.10Citation PageRank (#13467983 Global)
4Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A method is provided for the manufacture of a semi-planar silicon-on-sapphire composite comprising a sapphire substrate, an epitaxial monocrystalline silicon mesa formed adjacent the substrate and an epitaxial deposition of monocrystalline aluminum oxide surrounding the mesa. An essential step in the method is deposition of the aluminum oxide simultaneously adjacent the sapphire substrate and the monocrystalline silicon mesa whereby aluminum oxide formed adjacent the silicon mesa is polycrystalline and aluminum oxide deposited adjacent the sapphire substrate is monocrystalline. This enables the selective removal of the polycrystalline aluminum oxide adjacent the surface of the monocrystalline silicon mesa, thereby forming the composite.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 7.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for making a planar composite of at least one silicon island imbedded in single crystal aluminum oxide comprising the steps of: growing monocrystalline aluminum oxide adjacent an exposed surface of a substrate of sapphire and simultaneously growing polycrystalline aluminum oxide adjacent an exposed surface of an epitaxial island of silicon deposited on said substrate, by the pyrohydrolysis of aluminum trichloride, hydrogen, and carbon dioxide at a temperature between 875° C and 990° C, and selectively removing said polycrystalline aluminum oxide whereby a major surface of said island

  2. Claim 2Depends on #1

    A method according to claim 1 wherein the aluminum oxide depositions occur at a rate between 50 Angstroms and 400 Angstroms per minute.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗