Abstract

A considerable reduction in modulus, as well as a significant increase in scorch time of a carbon black-containing rubber composition is obtained if the carbon black has been previously oxidized with a very diluted aqueous nitric acid containing only about 0.05 to 1 wt. % of HNO 3 and dried at a temperature of about 400° to 550° F.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 15.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A process to produce oxidized carbon black which comprises contacting said carbon black with an aqueous nitric acid having a concentration of about 0.05 to about 1 weight % with the weight ratio of HNO 3 to carbon black being in the range of about 5 × 10 -4 to about 1 × 10 -2 and drying the thus treated carbon black at a temperature in the range of about 400° to about 550° F.

  2. Claim 2Depends on #1

    A process in accordance with claim 1 wherein said carbon black is contacted with said aqueous nitric acid in a pelleting mill.

  3. Claim 3Independent Claim

    A process for treating carbon black so as to adjust and control the modulus and/or scorch time of a rubber composition containing said carbon black which comprises a. compounding a sample of said carbon black and a rubber into a rubber composition, b. determining the modulus and/or scorch time of said rubber composi