Alkaline pulping of lignocellulosic material with amine and sulfate pretreatment
Abstract
A method is described for increasing the yield of pulp obtained from an alkaline pulping process. A lignocellulosic material, such as wood chips, is first pretreated with an aqueous solution containing from 0.1 to 10% by weight of monoethanolamine, methylamine or dimethylamine and from 0.01 to 1% by weight of copper sulfate or nickel sulfate at elevated temperature and pressure in a closed vessel. This pretreated material is then subjected to conventional alkaline pulping, preferably soda or two-stage soda-oxygen pulping.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 3.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
In a process for pulping raw lignocellulosic material, the steps which comprise first pretreating the lignocellulosic material with an aqueous solution containing from about 0.1 to 10% by weight of a water-soluble, low molecular weight aliphatic amine selected from the group consisting of monoethanolamine and methylamine and from about 0.01 to 1% by weight of a water-soluble transition metal salt selected from the group consisting of copper sulfate and nickel sulfate at elevated pressure in a closed vessel and thereafter subjecting the pretreated lignocellulosic material to an alkaline pulping
- Claim 2Depends on #1
A process according to claim 1 wherein the alkaline pulping process is a soda process.
- Claim 3Depends on #2
A process according to claim 2 wherein the digested lignocellulosic material is subjected to a second dige
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗