Ceramic materials
Abstract
Calcia-partially-stabilized zirconia ceramic materials which contain between 3.3 and 4.7 percent of calcia by weight. Such materials have a fine-scale two-phase microstructure substantially consisting of metastable, tetragonal domains of a critical size within cubic matrix grains, which domains, in regions of high stress, irreversibly transform to normal monoclinic form upon stressing of the body. The materials are produced by firing a zirconia body containing between 3.3 and 4.7 percent by weight of calcia at a temperature between 1700° C and 1950° C and allowing the body to cool at an average rate of at least 175° C per hour to a temperature within the range 1200° to 1450° C; followed by ageing with said temperature range for a time such that peak strength is obtained.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 45.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A refractory ceramic consisting essentially of a calcia-partially-stabilised zirconia body, and characterised in that the calcia concentration lies in the range 3.3-4.7 percent by weight of the ceramic body, and in that said body has a fine-scale two-phase microstructure substantially consisting of metastable, tetragonal domains of a critical size within cubic matrix grains, which domains, in regions of high stress, irreversibly transform to normal monoclinic form upon stressing of the body.
- Claim 2Depends on #1
A ceramic as claimed in claim 1, wherein the calcia content is in the range 3.4 to 4.2 percent by weight.
- Claim 3Depends on #1
A ceramic as claimed in claim 1, wherein the calcia content is about 4% by weight.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 45 total)
References Cited — Backward Prior Art (3)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 3,620,781 A | Partially stabilized zirconia refractory | 1971 | 22 |
| US 3,887,387 A | Shaped zirconium oxide bodies of high strength | 1975 | 35 |
| US 3,929,498 A | Sintered zirconia bodies | 1975 | 13 |