Process for producing cobalt- and iron-containing ferromagnetic powder by heat-treatment in the presence of an oxidizing agent
Abstract
A Co- and Fe-containing ferromagnetic iron oxide powder having a high coercive force and improved stability to heat and pressure is produced by adding an aqueous alkali solution, an aqueous solution containing Co +2 ions, and an aqueous solution containing not more than 1 equivalent, based on the Co +2 ions, of Fe ions to a suspension of ferromagnetic iron oxide, and heating the mixture at a temperature of at least 80° C in the presence of an oxidizing agent. The ferromagnetic iron oxide powder is especially suitable for producing magnetic recording media.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 19.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A process for producing a Co- and Fe-containing ferromagnetic iron oxide powder which comprises adding to a suspension of an acicular ferromagnetic iron oxide an oxidizing agent, an aqueous alkali solution, an aqueous solution containing Co +2 ions and an aqueous solution of Fe ions and heat treating the resultant mixture, at a temperature of at least about 80° C said CO +2 ions being present in said aqueous solution containing Co +2 ions in an amount of 0.5 to 10 atomic percent based on the amount of iron present in the acicular ferromagnetic iron oxide, said Fe ions being added to the sus
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 19 total)
References Cited — Backward Prior Art (6)
Non-Patent Literature (1)
- Umeki, "Chem. Abstracts," vol. 82, 1975, 79751v.