Magnesium reclamation process and apparatus
Abstract
A magnesium reclamation process whereby magnesium and magnesium alloy fines, chips and scraps may be recovered and remelted for reuse. The method is comprised of the steps of pelletizing the magnesium by first compacting the magnesium with a low pressure press so as to initially expel the majority of the air, followed by a high pressure press under a controlled environment to form a compact pellet. The pellets are then melted either by stacking on the cold heel of a pot and heating under a controlled environment or pre-heating in a basket over a melt, and then subsequently immersing the load. Melting can also be accomplished by controlled melting, utilizing an induction melting furnace whereas temperature can be slowly increased. Pelletizing pressures range from approximately the yield pressure to the cold welding pressure of the material being reclaimed. A typical pelletizing environment is 20% SF 6 and 80% CO 2 and a suitable melting environment is 98% CO 2 and 2% SF 6 .
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 18.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of compacting magnesium fines, chips and scraps comprising the steps of: a. placing the magnesium in the confined chamber of a press, b. pressing the magnesium at a low pressure to collect the magnesium at one end of the confined chamber and to expel a substantial portion of the air in the chamber, c. withdrawing the pressing element while providing an inert atmosphere in the increasing chamber volume, and d. pressing the magnesium at a high pressure to concentrate the magnesium into a self supporting pellet.
- Claim 2Depends on #1
The method of claim 1 comprised of the further step of releasing the pressure on the pressing element, opening the end of the chamber opposite the pressing element, and advancing the pressing element to eject the pellet.
- Claim 3Depends on #1
The method of claim 1 wherein said low pressure is less than 15,000 psi.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗