Patents
US 4,064,217 A#29867692 Most CitedExpiredUnited States (USPTO)Utility

Process for recovering aluminum from alunite ore

3Forward Citations (#29867692 Global)
0.1/yrCitation Velocity (#51722219 Global)
1.27Citation PageRank (#29665016 Global)
5Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

An improvement in the process for recovering aluminum from alunite ore disclosed in U.S. Pat. Nos. 3,890,425 and 3,890,426, the improvement being in the recovery of potassium sulfate by crystallization from the leaching solution resulting from potassium hydroxide leaching of the roasted ore, the improvement consisting of adding potassium hydroxide to the concentrated leach liquor prior to crystallization to increase the concentration of the potassium ion so that increased recoveries of potassium sulfate are obtained at a given temperature over those obtained when this procedure is not used. By this procedure a yield is obtained at a temperature below that which is required to obtain the same yield when potassium hydroxide is not used so that the high temperatures formerly necessary to hold enough potassium sulfate in solution for an economic crystallization are avoided. The improvement is particularly adapted to the process of the patents using potassium hydroxide as the leaching agent and in which the mother liquor is recycled to the leach as potassium hydroxide in an amount up to that required for the leaching step can be added in the crystallization step so that the potassium hy

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 3.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for recovering aluminum values for alunite ore comprising the steps of: a. leaching the alunite ore with potassium hydroxide and recovering a liquid portion containing compounds of sulphur and alkali metals, including potassium sulfate and a residue portion containing aluminum values; b. adding an effective amount of potassium hydroxide to the liquid portion recovered from step (a) to raise the concentration of potassium ion in said liquid for increasing the recovery of potassium sulfate at a given temperature; c. precipitating potassium sulfate from said liquid of step (b) and r

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗