US 4,061,802 A#2025139 Most CitedExpiredUnited States (USPTO)Utility

Plating process and bath

32Forward Citations (#2025139 Global)
0.7/yrCitation Velocity (#12155323 Global)
5.91Citation PageRank (#2526329 Global)
5Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

An electroless nickel bath for applying a nickel coating to articles without heat distortion, especially plastic articles, comprising water, nickel ions, a reducing agent for reducing the nickel ions to a metal, and a stabilizing agent for controlling the operating speed of the reducing agent, the bath being maintained at an alkaline pH, with the weight of the nickel ions being less than the weight of the hypophosphite anions. The nickel ions may be obtained from nickel salts, the reducing agent may be sodium hypophosphite, and the stabilizing agent may be sodium citrate and ammonium chloride. A replenish mixture for maintaining the bath comprising nickel ions and reducing agent anions in about the same ratio as in the original bath, and a stabilizing agent in about one-third the amount as in the original bath. A method of applying a nickel coating to articles comprising immersing the articles in said electroless nickel bath at room temperature.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 32.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    An electroless nickel bath for applying a nickel coating to articles comprising about 3/4 gallon of water, about 320 cc. of ammonium hydroxide, about 31/4 ounces of nickel sulphate, about 8 ounces of nickel chloride, about 12 ounces of sodium hypophosphite to provide the reducing agent anions for reducing the nickel ions to a metal and about 191/4 ounces of sodium citrate and about 131/2 ounces of ammonium chloride as the stablizing agent for controlling the operating speed of the reducing agent, the bath having a pH of about 8.5, and the ratio by weight of nickel ions to reducing agent anions

  2. Claim 2Independent Claim

    An electroless nickel bath for applying a nickel coating to articles at low temperatures so that the articles do not distort from heat, comprising the following approximate ingredients and ratios per liter of solution, 25.0 gr.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗