High-temperature glass composition
Abstract
Aluminosilicate glasses containing BaO and CaO are provided having combined high softening points along with exceptionally low liquidus temperatures. These glasses are within the following compositional limits in percent by weight: ______________________________________ Percentage Oxides Range ______________________________________ SiO 2 55-68 Al 2 O 3 15-18 CaO 7-13 BaO 6-16 ______________________________________ except for incidental impurities, residual fluxes and refining agents. The weight ratio of Al 2 O 3 to combined weight ratio of CaO and BaO in the present glass composition is maintained in the range 0.6:1 to 1:1. Such glasses provide an improved hermetic seal for high temperature lamp envelopes.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 40.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A molybdenum seal glass composition which consists essentially of oxides in approximate percent by weight 55-68 SiO 2 , 15-18 Al 2 O 3 , 7-13 CaO, and 6-16 BaO, along with minor amounts of incidental impurities, residual fluxes, and refining agents, wherein the weight ratio of Al 2 O 3 to combined weight ratio of CaO and BaO is about in the range 0.6:1 to 1:1 so as to reside in the eutectic region of this aluminosilicate system, said glass composition having a liquidus temperature no greater than about 1250° C, a strain point of at least about 725° C, and an average coefficient of linear th
- Claim 2Depends on #1
A glass composition as in claim 1 which is essentially alk