Grafting of silane on thermoplastics or elastomers for purposes of cross-linking
Abstract
Granulated polyethylene is agitated and mixed with a solution of silane with peroxide, activators and anti-oxidants and at a temperature between 80 DEG to 100 DEG C to obtain diffusion of these additives into the polyethylene particles which is followed by grafting through extrusion or radiation which in turn is followed by exposure to and/or development of water to obtain cross-linking. A catalyst is added preferably by mixing polyethylene powder with the catalyst and adding that powder to the powder with diffused silane, after that diffusion has been completed.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 45.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
In a method for providing a sheathing of cross-linking thermoplastic or elastomeric material, wherein the powdery or granular material is mixed with silane to be diffused into the material under conditions of obtaining a homogenic mixture and wherein the silane is grafted upon the molecules of the material, the improvement of adding water-containing additives to the mixture, and extruding a sheath, the water being released at an elevated temperature pursuant to the extrusion to cause cross-linking of the silane grafted material in the presence of moisture.
- Claim 2Depends on #1
Method as in claim 1, including adding about 0.05 to 5 parts (by weight) per 100 parts fluidizable polymer, of additives which develop water on decompositioning.
- Claim 3Depends on #2
Method as in claim 2 wherein the additive is a polyvinyl alcohol.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 45 total)
References Cited — Backward Prior Art (2)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 3,644,315 A | Moisture-curable polymers | 1972 | 37 |
| US 3,830,872 A | Use of xylene in controlling melt flow of modified polyolefin compositions | 1974 | 14 |