Method of forming silicon solar energy cell having improved back contact
Abstract
A silicon solar energy cell having a diffusant junction extending inwardly from one surface, an aluminum-silicon junction of the opposite polarity extending inwardly from the other surface, and a film of aluminum-oxygen-diffusant formed over the aluminum-silicon junction. The structure is formed by diffusing an unprotected wafer, coating the diffusant glass so formed on one side of the wafer with aluminum, and heating the wafer.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 16.
Claims (2 — 2 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of forming a silicon solar energy cell having junctions of opposite polarities, comprising heating a crystalline silicon wafer with a diffusant to form a front junction in a zone extending inwardly from the front surface of the wafer, a back junction extending inwardly from the back surface of the wafer and films of diffusant glass on said front and back surfaces, applying a coating of aluminum to the diffusant glass on the back surface of the wafer, and heating the wafer at a sufficient temperature until the aluminum has negated the polarity of the back junction and formed an aluminu
- Claim 2Independent Claim
A method as claimed