An improved ternary brass alloy includes silicon as the additive material and may be fabricated to provide a beta brass or a mixed alpha plus beta brass material. The composition limits of the constituents of the beta brass are fixed by two factors: (1) the M s or Martensite transformation temperature must be determined, and (2) the brass must be a totally beta phase above 454° C. The composition is betatized, that is, heated at approximately 800° C. and quenched at a fast rate so that the total beta phase is retained in order to provide material having a shape memory effect, a low spring back coefficient and super elastic properties. A continuous betatizing and quenching process may be utilized in the manufacture of strip and sheet products. Alternatively, specific compositions may be cold worked to provide a material having a low spring back coefficient and other improved physical characteristics. The alpha plus beta brass includes 25% to 75% by weight beta phase mixed with alpha phase. The gamma phase is not tolerated. Generally, the same composition limits as the beta brass material are observed through processing and characteristics of the mixed alpha plus beta are distinct. M

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 1 · Forward citations: 72.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for making an improved ternary brass alloy that includes silicon as an additive material comprising the steps of: preparing a substantially homogeneous, polycrystalline mix of 25% to 40% by weight zinc, 0.25% to 3.0% by weight silicon and the balance copper; alternately cold rolling and intermediate annealing said alloy; said annealing being in the range of 400° C. to 550° C. to soften said alloy and produce a continuous matrix of alpha phase material with uniformly distributed beta phase material including a minimum of about 25% beta phase material and a maximum of about 75% alph

  2. Claim 2Independent Claim

    A method of making an improved ternary brass alloy that includes silicon as an additive material comprising the steps of: preparing a substantially homogeneous polycrystalline mix of 25% to 40% by weig

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (1)

PatentTitleYearCitations
US 3,783,037 ATreatment of alloys197443