Enhancing magnetic properties of amorphous alloys by annealing under stress
Abstract
A nickel based amorphous alloy in elongated ribbon form is subjected to a stress in the range of 20 to 40 kilograms per square millimeter, and is heated to temperatures below the melting point, preferably in the range of 200° C. Such heating under stress is maintained for a period of time, whereupon the material is cooled. There results a residual enhancement of the magnetic properties which occur by application of stress, but which are extinguished when the stress is removed.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 26.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of providing a magnetically responsive metal comprising: selecting a sample from the class of amorphous magnetic metallic alloys; subjecting said sample to a controlled predetermined elastic stress; heating said sample in a stressed condition to a predetermined temperature; maintaining said sample in said heated state for a predetermined duration; cooling said sample; and removing said stress; whereby the remanence of said sample is substantially increased and the coercivity of said sample is substantially decreased.
- Claim 2Depends on #1
A method as described in claim 1 wherein said temperature in said heating step is sufficiently below the melting point of said sample such that the amorphous structure of said sample is retained.
- Claim 3Depends on #1
A method as described in claim 1 and further including, after said removing step, the
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗