US 4,052,273 A#8067870 Most CitedExpiredUnited States (USPTO)Utility

Method of anodizing porous tantalum

12Forward Citations (#8067870 Global)
0.2/yrCitation Velocity (#30252187 Global)
3.36Citation PageRank (#6315407 Global)
7Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method of anodizing porous tantalum material suitable for making a porous tantalum capacitor pellet or slug having decreased current leakage is described. After a pellet is anodized at a maximum predetermined desired voltage, it is removed from the anodizing bath and heated to a temperature of between 150° C. and 300° C. The pellet is maintained at such temperature for at least three minutes and then returned to the anodizing bath, at least once, and subjected to more electrical current.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 12.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    The method of anodizing a porous tantalum pellet comprising the steps of providing a porous tantalum pellet, preparing an anodizing bath of an aqueous nitric acid solution, disposing said pellet in said anodizing bath, passing an electrical current of up to 90 ma. per gram of pellet weight through said pellet for a period of at least 30 minutes, said current being substantially constant until a predetermined desired voltage is reached and thereafter said voltage remaining substantially constant, removing said pellet from said bath, heating said pellet to at a temperature of between 1

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • "The Surface Treatment of Aluminum" by S. Wernick et al., 3rd edition, Draper Ltd., Teddington, England, 1964, pp. 269-271, 348, 520-524.