Patents
US 4,052,201 A#1157165 Most CitedExpiredUnited States (USPTO)Utility

Amorphous alloys with improved resistance to embrittlement upon heat treatment

44Forward Citations (#1157165 Global)
0.9/yrCitation Velocity (#7900313 Global)
26.11Citation PageRank (#213876 Global)
3Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

An improvement in resistance to embrittlement upon heat treatment of amorphous metal alloys containing iron, nickel, cobalt and/or chromium in the temperature range of about 200° to 350° C is achieved by including boron or boron plus at least one metalloid element of carbon, silicon and aluminum in a total amount of about 15 to 25 atom percent of the alloy composition.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 44.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    An amorphous metal alloy that is at least 50 percent amorphous, characterized in that the alloy consists essentially of one of the compositions selected from the group consisting of Fe 77 B 15 C 5 Si 1 Al 2 , Fe 66 Cr 12 B 15 C 5 Si 2 , Fe 60 Cr 18 B 15 C 5 Si 2 , Fe 30 Ni 30 Co 20 B 18 Si 2 , Fe 28 Ni 30 Co 20 B 16 Si 4 Al 2 , Fe 28 Ni 28 Co 20 B 18 C 2 Si 2 Al 2 , Fe 28 Ni 30 Co 20 B 18 C 2 Al 2 and Fe 30 Ni 30 Co 20 B 17 Al 3 , said alloy being resistant to embrittlement upon heat treatment in the temperature range of about 200° to 325° C for at least 5

  2. Claim 2Independent Claim

    An amorphous metal alloy that is at least 50% amorphous, characterized in that the alloy consists essentially of the composition M' a B b , where M' is at least three elements selected from the group consisting of iron, ni

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗