A method for making a supported Raney nickel catalyst by coating a nickel substrate with aluminum or aluminum-nickel alloy, heat treating the coated substrate above the melting point of aluminum but below 1133 DEG C, quenching at a temperature below 854 DEG C to form NiAl3 as a solid phase in the substrate. The Raney nickel alloy coating is activated in the usual manner by leaching with sodium hydroxide solution.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 46.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A process for making a Raney nickel catalyst comprising: dipping a nickel support or substrate into a bath comprising molten aluminum; removing the support from the bath of molten aluminum, the said support now being coated with a layer of aluminum to form a specimen; heat treating the specimen in the absence of oxygen at a temperature of from about 700° to 1133° C.; and quenching the heat treated specimen at a temperature of from about 640° to 854° C. in the absence of oxygen to form NiAl 3 as a solid phase coating on the substrate; and leaching the coated substrate with sodium hydroxi

  2. Claim 2Depends on #1

    The process of claim 1 wherein the aluminum contains up to 30 percent by weight of nickel.

  3. Claim 3Depends on #1

    The process of claim 1 wherein the nickel support or substrate is