Low coercivity iron-silicon material, shields, and process
Abstract
Iron-silicon is sputtered onto a substrate to be used for a magnetic recording head from a target containing 4% to 7% of silicon with a substrate bias between -2.5 and -60 volts, anode-cathode spacing of about 1/2 to about 2 inches, a deposition rate of greater than 150A/min, a substrate temperature above 250° C, an argon pressure above 10 microns, and a single film thickness greater than 0.4 micron, a laminated film thickness greater than 0.05 micron, and R.F. input power above 8 watts/in 2 .
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 17.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A substrate having deposited thereon a thin film of iron-silicon made by the process comprising the steps of: placing a substrate upon the anode of an R.F. sputtering chamber, placing a target of iron-silicon containing about 4% to 7% silicon upon the cathode of said sputtering chamber, spacing said cathode and said anode about 1/2 inch to 2 inches apart, impressing an R.F. potential greater than 1200 volts upon said cathode for sputtering material from said target of iron-silicon at a rate greater than 150A/min onto said substrate to a thickness greater than 1/2 micron upon the said sub
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 17 total)
References Cited — Backward Prior Art (4)
Non-Patent Literature (2)
- H. Hieber, "On the Electron Microprobe Analysis of Structured Magnetic Thin Films," Thin Solid Films, 12, 29-34 (1972).
- I. Pockrand et al., "Magnetic Domains in Thin Sputtered FeSi Films," Phys. Stat. Sol. (a) 27, 413 (1975).