Two stage sulfuric acid leaching of sea nodules
Abstract
A process for extracting metal values from manganiferous sea nodules is provided in which nickel, copper, and cobalt values are selectively leached in a sulfuric acid medium in two stages, the first stage being effected at a temperature up to about 100° C and to a final pH of not less than about 1.5 and the second stage being effected at a temperature of about 160° C to about 260° C and at an initial pH of not less than about 1.5.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 30.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A two-stage process for treating manganiferous sea nodules containing acid soluble gangue minerals, a major amount of manganese and iron, and a minor amount of at least one of the nonferrous metals nickel, cobalt, and copper, for the selective extraction of said nonferrous metal values comprising: a. effecting a first stage leach of raw sea nodules slurried in a sulfuric acid medium at an elevated temperature up to about 100° C., said slurry having a pulp density of about 10% to 40% solids and having a sulfuric acid content of about 20% to 50% based on the weight of the nodules, the acid being
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 30 total)
References Cited — Backward Prior Art (5)
Non-Patent Literature (1)
- Perry et al. Chemical Engineering Handbook, 4th Edition McGraw-Hill Book Company (1963) pp. 11-25, 11-26.