US 4,045,368 A#805703 Most CitedExpiredUnited States (USPTO)Utility

Process for production of activated carbon spheres

54Forward Citations (#805703 Global)
1.1/yrCitation Velocity (#5766906 Global)
9.31Citation PageRank (#1194501 Global)
8Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Microporous pitch spheres prepared from pitch are oxidized at a temperature of from 100° C to 500° C in an atmosphere of an oxidative gas to produce pitch spheres containing not less than 10% by weight of combined oxygen. Then the combined oxygen-containing pitch spheres are heated at a temperature of from 150° C to 700° C in an atmosphere of ammonia gas to produce pitch spheres containing not less than 1.5% by weight combined nitrogen. The resultant pitch spheres are subsequently activated by a conventional method to produce activated carbon spheres containing more than 1% by weight of combined nitrogen.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 54.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for the production of activated carbon spheres, comprising: melting 100 parts by weight of a pitch in the presence of 10 to 50 parts by weight of naphthalene or tetralin to form a molten mixture; shaping said molten mixture into the form of spheres; contacting said spheres with a second solvent, said second solvent being compatible with the aromatic solvent, but lacking affinity for the pitch, to extract said aromatic solvent and to form microporous spheres; oxidizing said microporous spheres by heating said spheres at a temperature of from 100° C to 400° C in the presence of a