US 4,045,241 A#5535085 Most CitedExpiredUnited States (USPTO)Utility

Synthetic taeniolite and process of producing the same

16Forward Citations (#5535085 Global)
0.3/yrCitation Velocity (#22557361 Global)
6.46Citation PageRank (#2185985 Global)
2Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

This invention relates to a process of producing taeniolite having the formula, LiMg 2 Li(X 4 O 10 )F 2 (wherein X represents Si or Ge), which comprises mixing (a) lithium compound selected from the group of lithium oxide and lithium fluoride, (b) magnesium compound selected from the group of magnesium fluoride and magnesium oxide and (c) silicon oxide (or germanium oxide) in such a manner that the mixing ratio of Li : Mg : Si : (or Ge) : F becomes 1 : 1 : 2 : 1 (the fluoride is included in an excess amount of 10 - 30% to compensate the loss of fluorine during the process); melting the mixture at about 1,250° C-1,450° C and slowly cooling until the melt crystallizes. This invention further relates to a water sol of flake-like ultra-fine particles of taeniolite produced in accordance with the above mentioned process, wherein each flake-like particle dispersed in water has a thickness of less than 150 A and a ratio of a diameter of the flat plane of the flake/the thickness of the flake being more than 100/1.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 16.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A process of producing taeniolite having the formula, LiMg 2 Li(X 4 O 10 )F 2 wherein X represents Si or Ge, which comprises mixing (a) a lithium compound selected from the group of lithium oxide and lithium fluoride, (b) a magnesium compound selected from the group of magnesium fluoride and magnesium oxide and (c) silicon oxide or germanium oxide in such a manner that the mixing ratio of Li : Mg : Si or Ge : F becomes 1 : 1 : 2 : 1, the fluoride being included in an excess amount of 10- 30% to compensate for the loss of fluorine during the process; melting the mixture at 1,250° - 1,450° C.

  2. Claim 2Depends on #1

    A water sol of flake-like ultra-fine particles of taeniolite produced in accordance with claim 1, wherein each flake-like particle dispersed in water has a thickness of less than 150 A and a ratio of

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗