Removing crust of oxide from profiled wire rod
Abstract
Removing the crust of oxide formed on the surface of a continuously casted copper bar by projecting a liquid (water or a rolling emulsion) under pressure of between 20 and 60 atmospheres against the periphery of the bar, the flow of the liquid under pressure being less than 50 liters/minute.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 15.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
In the known process for the direct and continuous manufacture of copper wire rod starting from liquid metal, in which a bar is produced by continuous casting and conveyed while still hot to a rolling mill where the bar is rolled down into a wire rod in a plurality of roll passes, including a few early roll passes and several later roll passes, and in which process a crust of oxide is present on the surface of the rod being rolled down, the improvement which comprises removing the crust of oxide in at least one cleaning operation between the early roll passes by projecting a liquid selected fr
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗