Strengthening reaction sintered silicon nitride
Abstract
The strength of a reaction sintered silicon nitride body is substantially increased by impregnating the surface of the body with finely divided alumina and then firing the body in a nitrogen atmosphere to a temperature in excess of 1200° C, the reaction being carried out under an appreciable partial pressure of SiO.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 13.
Claims (3 — 2 Independent, 1 Dependent)
- Claim 1Independent Claim
In a process for increasing the strength of a previously formed reaction sintered silicon nitride body wherein the surface of the formed body is impregnated with a aluminum oxide (Al 2 O 3 ) and fired in a nitrogen atmosphere at a temperature between about 1200° and about 1500° C., the improvement which comprises maintaining a substantial partial pressure of SiO in the atmosphere during said firing.
- Claim 2Independent Claim
In a process for increasing the strength of a previously formed reaction sintered silicon nitride body wherein the surface of the formed body is impregnated with aluminum oxide and fired in a nitrogen atmosphere at a temperature above 1200° C., the improvement which comprises maintaining a substantial partial pressure of SiO in the atmosphere during said firing.
- Claim 3Depends on #1
The process of claim 1 wherein the partial press