Copper base alloy containing titanium, antimony and chromium
Abstract
Copper base alloys which exhibit a combination of high electrical conductivity and superior strength properties are presented. These alloys consist essentially of 0.08 to 1.0% by weight of titanium, 0.05 to 1.5% by weight of antimony, 0.1 to 1.0% by weight of chromium, balance copper. The desired properties are attained by the proper application of mechanical processing steps and thermal treatments.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 3.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A high conductivity and high strength copper base alloy consisting essentially of 0.08 to 1.0% by weight titanium, 0.05 to 1.5% by weight antimony, 0.1 to 1.0% by weight chromium, balance copper, wherein the titanium and antimony are present at an atomic ratio of not more than 10% above 5 atoms of titanium per 3 atoms of antimony.
- Claim 2Depends on #1
An alloy according to claim 1, wherein the titanium and antimony are present at an atomic ratio of 3 to 3.6 atoms of antimony per 5 atoms of titanium.
- Claim 3Depends on #1
An alloy according to claim 1, wherein the chromium is present in the alloy in an amount from 0.1 to 0.6% by weight.