Patents
US 4,035,191 A#2777497 Most CitedExpiredUnited States (USPTO)Utility

Tetragonally stabilized zirconia ceramic

26Forward Citations (#2777497 Global)
0.5/yrCitation Velocity (#14828804 Global)
8.11Citation PageRank (#1501081 Global)
3Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Mature zirconia ceramic compositions stabilized in the monoclinic and tetragonal structure with 0.1-5% ZnO and as little as 0.5% of a primary stabilizer selected from MgO, Y 2 O 3 or combinations thereof. Compacted ceramic compositions are fired and matured at temperatures below the volatilization point of ZnO and in the range of 2750°-2950° F. Zirconia is conventionally batched with magnesia, yttria or mixtures thereof, with or without other known stabilizers including ceria and calcia, together with up to about 5% ZnO and then compacted and sintered at a temperature which retains at least 0.1% ZnO in the fired body. Conventional cooling is prescribed. Subsequent thermal cycling of the fired body between 400° and 2500° F. reveals a stable body with no degradation in strength. Magnesia stabilized compositions show no signs of early destabilization on thermal cycling and may even show increasing room temperature strength as cycling progresses.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 26.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A mature, tetrastabilized zirconia fired composition consisting essentially of, by weight on the oxide basis, 0.1-5.0% ZnO and at least 0.5% of a primary stabilizer selected from 0.25% up to less than about 4% MgO, 0.25% up to less than about 4% Y 2 O 3 and combinations thereof, the balance substantially being ZrO 2 , said fired composition having less than 10% cubic structure and at least 5% tetragonal structure by volume at room temperature.

  2. Claim 2Independent Claim

    A method of producing a tetrastabilized zirconia fired composition having less than 10% cubic structure and at least 5% tetragonal structure at room temperature and being characterized by a retained strength upon thermal cycling below 2,900° F. comprising, (a) blending a raw material batch consisting essentially of, by weight on the oxide basis 0.1-5.0% ZnO, at least 0.5% of a primary stabilizer se

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗