Grain-oriented silicon steel and processing therefor
Abstract
A process for producing grain-oriented silicon steel, and the steel produced thereby. The process includes the steps of: preparing a melt of silicon steel; casting the steel; hot rolling the steel; cold rolling the steel; decarburizing the steel; final texture annealing the steel; coating the steel with an aqueous solution comprised of from 4 to 30% of phosphate ion, up to 6% magnesium ion, 5 to 34% colloidal silica and 0.15 to 6% hexavalent chromium; and curing the coated steel at a temperature of at least 1200° F.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 11.
Claims (3 — 2 Independent, 1 Dependent)
- Claim 1Independent Claim
As an article of manufacture, grain-oriented silicon steel having a cube-on-edge orientation and a cured coating thereon, said coating having been formed from an aqueous solution consisting essentially of from 4 to 30% phosphate ion, 0.3 to 6% magnesium ion, 5 to 34% colloidal silica, 0.15 to 6% hexavalent chromium, balance water; said cured coating placing said steel in tension, said tension being at least 800 psi.
- Claim 2Depends on #1
An article according to claim 1, wherein said tension is at least 1200 psi.
- Claim 3Independent Claim
In a process for producing grain-oriented silicon steel, which process includes the steps of: preparing a melt of silicon steel; casting said steel; hot rolling said steel; cold rolling said steel; decarburizing said steel; and final texture annealing said steel; the improvement comprising the steps of coating said annealed steel
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗