Pyrometallurgical recovery of copper from slag material

12Forward Citations (#7920659 Global)
0.2/yrCitation Velocity (#30224469 Global)
6.30Citation PageRank (#2277339 Global)
8Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A cyclic, two-stage process is disclosed for pyrometallurgical recovery of copper as a high-grade matte from molten slag material containing both dissolved and/or entrained copper values. A charge of the copper-bearing slag material is treated in the first stage of the process with a hydrocarbonaceous or hydrogenous reductant in a rotary furnace, such as a top-blown rotary reactor, rotating at at least about 10 rpm, to form a high-grade copper matte phase and a slag phase of reduced copper content. The rotation of the reactor is discontinued and the high-grade copper matte phase separates from the slag phase and is recovered from the reactor. The reactor containing the remaining slag of reduced copper content is again rotated at about 10 rpm, and iron sulfide, e.g. pyrite, is added in the second stage of the process to the slag in the rotating reactor to provide a low-grade matte phase which literally "washes out" most of the remaining copper contained in the slag. The rotation of the reactor is again discontinued and the low-grade matte phase separates from the remaining slag phase. The remaining slag phase is removed from the reactor, and the low-grade matte produced in t

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 12.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A cyclic, two-stage process for recovering essentially all copper values present in molten slag, comprising: (a) subjecting a charge of the molten slag to vigorous agitation in a rotary reactor rotating at a speed of at least about 10 rpm; (b) adding a carbonaceous or hydrogenous reductant to said charge of molten slag in the rotating reactor to reduce magnetite and to produce a high-grade matte, containing at least about 70% copper, and a slag; (c) discontinuing rotation of the reactor, thereby allowing the high-grade matte to separate from the slag, whereby a matte phase and a slag phase are