Recovery of gallium
Abstract
This invention relates to an improvement in the well known "Bayer" process. In particular, the invention describes a process for the recovery of gallium and alumina from bauxite including the steps of: A. dissolving the ore in caustic soda solution under pressure; B. precipitation of pure alumina from the remaining caustic soda solution by reduction of temperature and pressure; C. subjecting the resulting mother liquor from (b) to an elevated temperature of 60° to 450° C and a pressure of 2 to 100 atmos. in the presence of an oxygen-containing atmosphere; and D. cementation of the gallium remaining in solution by contact with metallic aluminium. Step (a) is preferably carried out at a pressure of 5 atmospheres and step (c) is carried out in the presence of an atmosphere consisting substantially of oxygen at a pressure within the range 20 to 50 atmospheres and a temperature within the range 150° to 350° C. The metallic aluminium used in step (d) is preferably in the form of turnings or coarse filings.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 2.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A process for the recovery of gallium and alumina from bauxite ore comprising the steps of: a. dissolving the ore in caustic soda solution under pressure; b. precipitating alumina from the remaining caustic soda solution by reduction of temperature and pressure; c. subjecting the resulting mother liquor from (b) to an elevated temperature of 60° to 450° C and a pressure of 2 to 100 atmos. in the presence of an oxygen-containing atmosphere; and d. cementation of the gallium remaining in solution by contact with metallic aluminium.
- Claim 2Depends on #1
A process according to claim 1, wherein step (a) is carried out at a pressure of 5 atmospheres.
- Claim 3Depends on #1
A process according to claim 1, wherein step (c) is carried out in an atmosphere consisting substantially of oxygen at a pressure within 20 to 50 atmospheres and at a temperature
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (2 of 2 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| CN 1,982,018 B | Mold for tire | 2010 | 0 |
| WO 9,322,478 A1 | Electrolytic method of obtaining gallium metal | — | 0 |