Patents
US 4,028,484 A#9151924 Most CitedExpiredUnited States (USPTO)Utility

Alfin polymerized rubber

11Forward Citations (#9151924 Global)
0.2/yrCitation Velocity (#31141550 Global)
2.53Citation PageRank (#9992386 Global)
9Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The effectiveness of an alfin catalyst and the quality of the rubber it produces are increased by carrying out the polymerization in a closed container in which the ratio of vapor to liquid space is less than 0.2, this ratio being responsible for a reduction of the boiling (desorption of monomer) that occurs on each particle because of the heat of polymerization. In general the effectiveness of the catalyst and the quality of the polymer are improved by any method or combination of methods that reduces the boiling per particle to a level less than that achieved by carrying out the reaction in a closed container in which the volume of vapor space to liquid is less than 0.2. The more this reduction, the better the product as a rule. The product obtained is a millable rubber of high molecular weight, well above that of natural rubber and primarily with a trans structure of the diene component. This fact was demonstrated with a styrene:butadiene proportion of around 30:70, polymerized under a combination of influences that restrained boiling. The polymer compounded readily, that is to say, the rubber banded on a warm mill and compounded easily in a conventional recipe. Rubbers with an

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 11.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    An alfin catalyzed rubber, selected from the group consisting of butadiene homopolymer and butadiene-styrene copolymer, of DSV greater than 9 and which compounds as soft rubber on a rubber mill after no more than about 15 minutes of mixing in the presence of no more than about 15 phr processing oil added on the mill, and being dischargeable from the mill at a temperature of no more than about 145° C said rubber having been made by polymerization in a closed reaction chamber in which the internal pressure during reaction corresponds to a vapor/liquid ratio of less than about 0.2.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗