Composites consisting of sintered tungsten carbide particles in a local matrix of a steel alloy having a carbon, cobalt and tungsten content are prepared by placing particles of tungsten carbide with cobalt binder, at least some of which are larger in size than those desired in the final composite in a mold. Matrixing alloy having little or no tungsten content is heated above its melting temperature and then poured into the relatively cold mold. The carbon, tungsten and cobalt dissolve at the outer surfaces of the particles and diffuse into the alloy which is allowed to naturally cool and solidify.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 84.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
The method of forming a metal tungsten carbide composite comprising: supporting a plurality of cobalt bound tungsten carbide particles having a mesh size of an average size substantially larger than the tungsten carbide particles desired in the finished composite within a mold; separately heating a metal, to between 2800° F. and 3200° F.; pouring the metal into the mold while the particles are at a temperature below about 2200° F. and immediately allowing the mass to cool and solidify to cause solution of the sintered tungsten carbide into the metal from the surfaces of the particles and diffu
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗