Method of manufacturing a cerium activated luminescent rare-earth aluminate
Abstract
A method of manufacturing a rare-earth aluminate, particularly a luminescent rare-earth aluminate, in which a starting mixture of the composite oxides or of compounds producing these oxides at an elevated temperature together with a flux is heated at a high temperature. At least one of the compounds rubidium fluoride, cesium fluoride and potassium fluoride is used as a flux.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 14.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
In the method of manufacturing a luminescent rare earth aluminate selected from the group consisting of the cerium activated rare earth aluminates of the formula Ln 3 Al 5 O 12 and LnAlO 3 wherein Ln is at least one element selected from those having atomic numbers 57 to 71 inclusive and yttrium by heating a starting mixture of the oxides required to produce said aluminate or of compounds capable of producing such oxides upon being heated, together with a flux at a temperature of from about 1200° to 1400° C for about 0.5 to 4 hours the improvement wherein the flux is at least one compound
- Claim 2Depends on #1
The method of claim 1 wherein the flux is employed in a quant