Manufacture of glass using briquettes

46Forward Citations (#1096027 Global)
0.9/yrCitation Velocity (#7582614 Global)
5.57Citation PageRank (#2778238 Global)
20Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

An improved process is described for producing glass in which a glass batch is mixed with a binder, aged, compacted, and compressed into briquettes, which are heated to partially react the contents of the batch in a prereaction stage. Prereacted briquettes are then placed in a fuel-fired furnace and heated at a temperature not above 2,600° F (1,430° C) to refine them into glass.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 20 · Forward citations: 46.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for the continuous manufacture of glass from glass batch comprising silicon dioxide, soda ash and a calcium carbonate or calcium oxide in a glass furnace comprising: a. adding to the glass batch a binder selected from the group consisting of water and an aqueous caustic soda solution, in amounts up to 10% by weight of the batch, b. aging the glass batch and binder for a period of at least 10 minutes, c. compacting the glass batch and binder by compressing same in a prebriquetting stage, d. dividing the compacted glass batch and binder into particulate form, e. briquetting the

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • Manring; W. H. and W. C. Bauer, "The Batch Preparation Process-Past, Present and Future", The American Ceramic Society Bulletin, vol. 52, Aug. 1973.
  • Manring; W. H., "Discussion of Influence on Furnace Atmosphere on the Melting-Fining Rate of Soda Lime Glasses", Canadian Clay and Ceramics, Feb. 1973.