Method of obtaining copper from copper-bearing ores

27Forward Citations (#2642037 Global)
0.6/yrCitation Velocity (#14472510 Global)
6.00Citation PageRank (#2462632 Global)
5Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The invention provides a method for obtaining electrolytic copper from copper-bearing ores which involves (a) lixiviating a sulphurized copper concentrate with an aqueous solution containing cupric chloride; (b) separating the solution resulting from the lixiviation stage (a) into two parts, one of said parts, containing at least 1 gram of cuprous ions per liter and at least 2 grams of ferrous ions per liter, being subjected to oxidation by air at atmospheric pressure, at a pH value between 1 and 3, and at a temperature above 90° C., resulting in the precipitation of goethite [FeO(OH)] which is separated, and the resulting solution then recycled to the lixiviation stage (a); (c) partially extracting the copper contained in the other part of the solution resulting from the lixiviation stage (a) by contacting the solution with an organic phase containing a cationic solvent, this extraction being accompanied by oxidation by injection of air; (d) re-extracting the copper, now contained in the organic phase, by contacting the latter with an aqueous sulphuric acid solution and recycling the organic phase to extraction stage (c); and (e) treating the copper sulphate solution obtained from

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 27.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for obtaining electrolytic copper from copper-bearing ores comprising: a. lixiviating a sulphurized copper concentrate with an aqueous solution containing cupric chloride; b. separating into two parts the solution resulting from the lixiviation stage a), one of said parts, containing at least 1 gram of cuprous ions per liter and at least 2 grams of ferrous ions per liter, being subjected to oxidation by air at atmospheric pressure, at a pH-value of between 1 and 3 and, at a temperature above 90° C., with precipitation of goethite and separation thereof, the resulting solution then b

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • Kruger, Chemie-Ingenieur Techick, vol. 45, No. 4, (1973), pp. 154-157.