Patents
US 4,021,272 A#1282491 Most CitedExpiredUnited States (USPTO)Utility

Method of isothermal annealing of band steels for tools and razor blades

42Forward Citations (#1282491 Global)
0.9/yrCitation Velocity (#8355709 Global)
6.11Citation PageRank (#2388092 Global)
5Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method consisting in converting a coil of hot-rolled band steel for tools and razor blades into an open coil in which its convolutions are spaced apart from one another, and immersing the open coil in a series of salt baths. First of all, the open coil is immersed for 5 to 30 minutes in a salt bath held at a temperature in a range from 550° to 750° C. to preheat the open coil and cause preliminary precipitation of carbides. The preheated open coil is immersed for 5 to 30 minutes in a salt bath held at a temperature in a range from the temperature immediately above Acl point to the temperature of Acl point plus 50° C. to make the band steel austenitic in structure. The open coil is then immersed for over 10 minutes in a salt bath held at a temperature in a range from the temperature immediately below Arl point to the temperature of Arl point minus 80° C. so that the isothermal transformation may be completed. Finally, the open coil is immersed for 3 to 10 minutes in a salt bath held at a temperature in a range from 600° to 650° C. and air cooled thereafter. The method enables to produce band steels for tools and razor blades which contain carbides occurring in a small spheroidal s

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 42.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of isothermal annealing of a hot-rolled band steel selected from the group consisting of a tool steel and a stainless steel comprising the successive steps of: converting a coil of said hot-rolled band steel into an open coil with its convolutions spaced apart a distance great enough to allow a molten salt to pass therethrough; immersing said open coil in a molten salt bath held at a temperature in a range of from 550° to 750° C. for a period of 5 to 30 minutes to preheat the open coil and cause preliminary precipitation of carbides; immersing the preheated open coil in a molten s

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗