Patents
US 4,017,664 A#1111358 Most CitedExpiredUnited States (USPTO)Utility

Silicon carbide electrolyte retaining matrix for fuel cells

45Forward Citations (#1111358 Global)
0.9/yrCitation Velocity (#7712839 Global)
39.92Citation PageRank (#104543 Global)
3Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

In a fuel cell utilizing an acid electrolyte, such as H3PO4, the electrolyte retaining matrix is made from silicon carbide. The silicon carbide has been found to be virtually inert to H3PO4 at fuel cell operating temperatures and provides all the other necessary and desirable matrix properties. This matrix is expected to have a life of at least 40,000 hours under normal fuel cell operating conditions.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 45.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A fuel cell comprising: a pair of spaced apart gas diffusion electrodes; a porous electrolyte retaining matrix confined in the space between said electrodes and extending therebetween, and comprising at least 90% silicon carbide; and phosphoric acid electrolyte disposed within said matrix.

  2. Claim 2Depends on #1

    The fuel cell according to claim 1 wherein said matrix includes up to 10% binder.

  3. Claim 3Depends on #2

    The fuel cell according to claim 2 wherein said binder is a fluorocarbon polymer.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗