Polytetramethylene ether urethane cured with 2,2'-diaminodiphenyl disulphide

13Forward Citations (#7181414 Global)
0.3/yrCitation Velocity (#27249163 Global)
7.98Citation PageRank (#1543916 Global)
2Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

Polytetramethylene ether urethane having improved physical properties is produced by reacting polytetramethylene ether polyol with a toluene diisocyanate containing at least 50 percent 2,4 isomer, reacting at a temperature no greater than about 40 DEG C. to produce a prepolymer and curing the prepolymer with 2,2'-dithio dianiline having the formula <IMAGE> at a temperature of 105 DEG C.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 13.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A polytetramethylene ether polyol urethane prepared by reacting a mol of a polytetramethylene ether polyol having 2 to 3 hydroxyls and an average molecular weight of 1000 to 4000 with 1.6 to 4 mols of toluene diisocyanate containing at least 50 percent by weight of the 2,4 isomer at a temperature from ambient to 40° C. to form a prepolymer and curing said prepolymer at a temperature no higher than 150° C. with 0.8 to 0.95 mol percent of 2,2'-dithiodianiline.

  2. Claim 2Depends on #1

    The urethane of claim 1 wherein the polytetramethylene ether polyol has 2 hydroxyls.