Method of developing and stripping positive photoresist
Abstract
Baked novolak resin based positive photoresists are either developed after exposure or stripped, following the use of the pattern resist layer as an etch mask, in aqueous solutions of a combination of permanganate and phosphoric acid.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 50.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A method of forming a patterned resist mask on a substrate comprising coating a layer of novolak resin based positive photoresist comprising an alkali-soluble phenolformaldehyde novolak resin and a 1,2-diazide naphthoquinone sensitizer, on said substrate, selectively exposing said layer to actinic radiation through a patterned mask, subsequently baking said layer at a temperature between 130° and 210° C, and then developing said layer with an aqueous solution consisting essentially of between about 0.038 and 1.5 percent by weight of a permanganate and between about 2 to 30 percent by weight of
- Claim 2Depends on #1
The process of claim 1 wherein the aqeuous solution contains about 10% by weight phosphori
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 50 total)
References Cited — Backward Prior Art (11)
Non-Patent Literature (3)
- German et al., "J. of Photo Science", vol. 15, pp. 137-144, 5/1967.
- Kaplan et al., "IBM Technical Discl. Bulletin", vol. 14, No. 10, 3/1972.
- Kaplan, "IBM Technical Discl. Bulletin", vol. 13, No. 2, 7/1970.