Fast cooling styrene polymer foams
Abstract
Expandable styrene polymer particles which have fast cooling rates during molding are produced by dry blending styrene polymer particles in the presence of 0.05 to 0.4 parts of silicone surfactant per 100 parts of polymer particles. The silicone surfactant is selected from the siloxane-oxyalkylene copolymers having at least one polysiloxane block which contains mers of the general formula R 2 SiO, where R is selected from the group consisting of alkyl having 1 to 4 carbon atoms and halogenated alkyl having 1 to 4 carbon atoms, and at least one polyoxyalkylene block containing mers of general formula C n H 2n O, where n is 2, 3 or 4, attached to said polysiloxane block and terminated by acetoxy or alkyl ether groups.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 3.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
Method of making foamable styrene polymer articles which yield fast cooling foamed moldings of large cross-section consisting of intimately mixing a dry blend of a. styrene polymer particles containing 3 to 20 weight per cent of a blowing agent, and b. 0.05 to 0.4 weight percent of a silicone surfactant selected from the siloxane-oxyalkylene copolymers having (1) at least one polysiloxane block which contains mers of the general formula R 2 SiO where R is selected from the group consisting of alkyl having 1 to 4 carbon atoms and halogenated alkyl having 1 to 4 carbon atoms, and (2) at least
- Claim 2Depends on #1
The method of claim 1 wherein said styrene polymer particles