Method for making polyetherimide
Abstract
A method is provided for making polyetherimides involving the reaction of aromatic bis(etheranhydride)s and organic diamines in the presence of an inert nonpolar organic solvent at temperatures of at least 130° C. The polyetherimides are useful as injection molding compounds.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 1 · Forward citations: 37.
Claims (2 — 2 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for making polyetherimide which comprises 1. refluxing a mixture containing as essential ingredients an aromatic bis(ether anhydride) of the formula ##SPC8## an organic diamine of the formula H.sub.2 NR.sup.1 NH.sub.2 and an inert nonpolar organic solvent at temperatures of from 130° C to 300° C while continuously effecting the removal of water of reaction during the course of polymer formation and 2.
- Claim 2Independent Claim
separating said polyetherimide at the termination of the reaction from the resulting reaction mixture of (1), consisting essentially of said polyetherimide and said inert nonpolar organic solvent, where R is a member selected from the class consisting of (a) the following divalent organic radicals: ##SPC9## and (b) divalent organic radicals of
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 37 total)
References Cited — Backward Prior Art (1)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 3,699,075 A | Soluble high molecular weight polyimide | 1972 | 34 |