Yarn sizes, sizing treatments and resulting sized yarns
Abstract
Textile size compositions which are dispersible in water and comprise an alkali metal and/or ammonium salt of a styrene-maleic anhydride copolymer containing as a copolymerized component a diester of an olefinically unsaturated dicarboxylic acid or anhydride and a monohydric alcohol and/or a polyester of such an acid or anhydride and a polyhydric alcohol. Also, textile size compositions which are dispersible in water and comprise a mixed salt of a styrene-maleic anhydride copolymer, wherein 20 to 80 weight percent of the cations of said salt are ammonium cations and 20 to 80 weight percent of the cations of said salt are alkali metal cations. Methods for sizing yarns and yarn sized with the above-mentioned compositions.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 9.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for preparing and finishing textile materials which comprises: A. treating a textile material with an aqueous solution of a mixed salt of a copolymer, said copolymer comprising 0.67 to 1.0 molar proportion of maleic anhydride, and one molar proportion of at least one monovinyl aromatic monomer containing 8 to 12 carbon atoms, and wherein a. from 20 to 80% of the free carboxyl groups of said interpolymer are combined with at least one fixed base selected from the group consisting of alkali metal bases, and b. from 20 to 80% of the free carboxyl groups of said interpolymer are combine
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗