Vacuum brazing of nickel to aluminum
Abstract
A method for brazing nickel to aluminum in a vacuum and product produced thereby. The outer surface of the aluminum member to which the nickel member is to be brazed is precoated with a layer containing silicon and magnesium. The nickel and aluminum members are placed together in an oven at reduced pressures and heated to a temperature of approximately 593°C cracking the oxide coating upon the aluminum sheet. The presence of magnesium and silicon in the surface of the aluminum sheets makes possible an excellent braze with a large filleted area. The process may be further adapted for brazing other metal components to aluminum by first precoating the component with nickel.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 29.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
The method comprising the steps of: providing members or predominantly nickel and aluminum or alloy of aluminum; assembling said members in a preferred configuration; providing a brazing material at junctures between said members, said brazing material comprising aluminum, silicon, and magnesium; providing a non-reactive atmosphere around the assembled members; and heating said members until a braze forms therebetween.
- Claim 2Depends on #1
The method of claim 1 further comprising the step of lowering the temperature of said members at a predetermined rate.
- Claim 3Depends on #2
The method of claim 2 wherein said non-reactive atmosphere comprises a partial vacuum of no more than 10 - 4 torr.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 29 total)
References Cited — Backward Prior Art (6)
Non-Patent Literature (1)
- fenton, Ed. Brazing Manual pp. 31, 38, 39, 131 and 139 American Welding Soc. N.Y., N.Y. 1963.