Patents
US 3,977,918 A#1831426 Most CitedExpiredUnited States (USPTO)Utility

Method of making magnets

34Forward Citations (#1831426 Global)
0.7/yrCitation Velocity (#11144493 Global)
6.26Citation PageRank (#2299458 Global)
4Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method of making an integral toroidal magnet comprising the steps of compacting suitable magnetic powder material into a toroidal shape while subjecting it to a particle aligning magnetic field, hot pressing the compacted powder toroid in a confining die at a temperature and pressure sufficient to cause shrinkage of the toroid in the axial direction and provide a packing density greater than 93% of the theoretical maximum value and substantially unidimensional shrinkage, heat treating the toroid at a temperature sufficiently higher than the hot pressing temperature to achieve an enhanced crystallographic alignment equivalent to the alignment obtained by sintering, annealing the toroid at a temperature sufficiently lower than the heat treating temperature to provide a magnetic coercivity similar to the coercivity achieved by annealing after sintering, and magnetizing the heat treated toroid in the direction of crystallographic alignment.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 34.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of fabricating magnets from magnetic powder material comprising the steps of; hot pressing the powder material into a desired configuration at a temperature in the range of about 800° to about 1100°C, said hot pressing temperature being below the sintering temperature range of the material, and at a pressure in the range of about 1,000 to about 10,000 pounds per square inch, said pressure being sufficient to produce a packing density greater than about 93% of the theoretical maximum value; heat treating the hot pressed material at a temperature greater than 1100°C, said heat treatin

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 34 total)

PatentTitleYearCitations
US 4,541,925 AComposition and hydrotreating process for the operation of a magnetically stabilized fluidized bed19859
US 10,109,418 B2System and process for friction consolidation fabrication of permanent magnets and other extrusion and non-extrusion structures20183
US 12,365,027 B2High speed shear-assisted extrusion20250
US 4,367,153 AComposition for use in a magnetically fluidized bed198310
US 10,189,063 B2System and process for formation of extrusion products20191
US 10,695,811 B2Functionally graded coatings and claddings20200
US 4,564,400 AMethod of improving magnets19863
US 4,541,924 AComposition and hydrotreating process for the operation of a magnetically stabilized fluidized bed19856
US 11,534,811 B2Method for forming hollow profile non-circular extrusions using shear assisted processing and extrusion (ShAPE)20221
US 11,946,504 B2Assemblies, riveted assemblies, methods for affixing substrates, and methods for mixing materials to form a metallurgical bond20240
US 12,397,334 B2Shear-assisted extrusion assemblies and methods20250
US 4,541,920 AComposition and reforming process for the operation of a magnetically stabilized fluidized bed19857
FR 2,385,196 A1Procede de fabrication d'aimants incurves de faible epaisseur a partir de poudres d'alliages terre rare-cobalt—3
US 12,186,791 B2Devices and methods for performing shear-assisted extrusion and extrusion processes20250
US 11,684,959 B2Extrusion processes for forming extrusions of a desired composition from a feedstock20230