Bath and method for the electrodeposition of bright nickel-iron deposits

36Forward Citations (#1658913 Global)
0.7/yrCitation Velocity (#10515561 Global)
7.21Citation PageRank (#1824780 Global)
6Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A nickel-iron alloy plating bath containing nickel ions and iron ions, a soluble non-reducing complexing agent, and a reducing saccharide selected from the group consisting of monosaccharides and disaccharides. The combination of hydroxy carboxylic acid complexers and reducing saccharide in such baths yielding high iron content bright level nickel-iron alloy deposits containing up to 50 percent iron, while retaining the Fe + 3 concentration in the bath at a minimum value and reducing the amount of complexers which is required. Generally, it is preferred to utilize from about 1 to about 50 grams per liter of a reducing saccharide and from about 2 to about 100 grams per liter of the complexing agent.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 36.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    An aqueous acidic bath suitable for the electrodeposition of a bright iron-nickel electrodeposit onto a substrate susceptible to corrosion, which comprises iron ions and nickel ions, the ratio of nickel ions to iron ions being from bout 5 to about 50 to 1, an organic sulfo-oxygen compound as a bath soluble primary nickel brightener present in an amount of from about 0.5 to 10 grams per liter, and 2 to 100 grams per liter of a bath soluble complexing agent which is a hydroxy aliphatic carboxylic acid having 1 to 3 carboxyl groups, 2 to 8 carbon atoms and 1 to 6 hydroxyl groups, the ratio of com

  2. Claim 2Independent Claim

    In a method for the electrodeposition of

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 36 total)

PatentTitleYearCitations
DE 2,826,464 A1Verfahren zur galvanischen abscheidung eines eisen und nickel und/oder kobalt enthaltenden niederschlags und hierfuer geeignetes bad—0
US 4,129,482 AElectroplating iron group metal alloys197823
US 9,004,960 B2Connector with gold-palladium plated contacts20152
CN 111,094,633 AElectroplating solution for iron-nickel alloy having low thermal expansion coefficient and electroplating method using the same—0
US 4,179,343 AElectroplating bath and process for producing bright, high-leveling nickel iron electrodeposits197915
US 7,553,553 B2Article comprising a fine-grained metallic material and a polymeric material200922
WO 2013/000674 A1Electrolytic freezing of zinc surfaces—0
US 9,309,602 B2Electrolytic iron metallizing of zinc surfaces20161
KR 20200044860 A저열팽창 계수를 갖는 철-니켈 합금용 전기 도금액 및 이것을 사용한 전기 도금 방법—0
US 8,129,034 B2Fine-grained metallic coatings having the coeficient of thermal expansion matched to one of the substrate20124
US 7,910,224 B2Fine-grained metallic coatings having the coefficient of thermal expansion matched to the one of the substrate20115
US 4,462,874 ACyanide-free copper plating process198424
FR 2,448,584 A1Procede de production de depots electrolytiques nickel-fer et bains utilises dans ce but, renfermant notamment un tartrate et un mono ou un disaccharide reducteur—0
US 2006135282 A1Article comprising a fine-grained metallic material and a polymeric material—72
US 2010028714 A1Fine-Grained Metallic Coatings Having the Coefficient of Thermal Expansion Matched to the One of the Substrate—22