Process for texturing polyester yarn
Abstract
A process for draw-texturing polyester yarn which has been melt-spun at high speed. The process is performed on a conventional false-twist texturing machine modified for drawing and for the use of an air-jet texturing device instead of a second heater. The yarn is drawn at 1.3 to 2.0X draw ratio, false-twist textured, and then air-jet textured to provide a yarn having a low boil-off shrinkage, resiliency and spun-like aesthetics.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 17.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
In the process for producing textured polyester yarn wherein synthetic linear ethylene terephthalate polymer is meltspun into filaments at 3000 to 5000 yards per minute to form a yarn characterized by a break elongation of 70 to 180 percent, by a birefringence value of at least 0.025, and by polyester which is less than 30 percent crystalline and has a relative viscosity of at least 18, and the yarn is drawn and textured in a draw-twist zone of a false-twist texturing machine with a heater temperature of at least 180°C; the improvement which comprises draw-texturing the yarn at 1.3 to 2.0 draw
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 17 total)
References Cited — Backward Prior Art (9)
Non-Patent Literature (1)
- "Research Disclosure", --Apr. 1973; p. 29.