Abstract
A copper, zinc, aluminum and boron catalyst is used as a low temperature methanol synthesis catalyst. The proportions of the catalyst components, in terms of metal atoms, are 30-70% of copper, 15-50% of zinc, 1-16% of aluminum and 0.3-5.3% of boron. This catalyst is prepared by adding an alumina sol to the mixture of copper, zinc and boron compounds and firing the total mixture.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 17.
Claims (3 — 2 Independent, 1 Dependent)
- Claim 1Independent Claim
A catalyst suited for the production of methanol which comprises the oxides of copper, zinc, aluminum and boron, wherein the proportion of catalyst components is 30-70% Cu, 15-50% Zn, 1-16% Al and 0.3-5.3% B, all the percentages being expressed by the metal atom ratio.
- Claim 2Depends on #1
A catalyst as claimed in claim 1, wherein the proportion of catalyst components is 30-70% Cu, 15-50% Zn, 3-12% Al and 0.5-3.5% B, all the percentages being expressed by the metal atom ratio.
- Claim 3Independent Claim
A process for the preparation of a catalyst suited for the production of methanol, which comprises adding an alumina sol to the mixture of a water-soluble copper salt, a water-soluble zinc salt and a water-soluble boron compound selected from borax, ammonium borate or boric acid, and then firing the total mixture.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 17 total)
References Cited — Backward Prior Art (2)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 3,703,386 A | Nonflow solder-stop glasses comprising lead-zinc borate and ceramic | 1972 | 14 |
| US 3,790,505 A | Low temperature methanol synthesis catalyst | 1974 | 26 |