Low melt index ethylene-vinyl acetate copolymers
Abstract
The melt index of ethylene-vinyl acetate copolymers is decreased by mechanically working the preformed copolymers.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 5.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A process for decreasing the melt index of preformed ethylene-vinyl acetate copolymers having about 8-55 weight percent vinyl acetate to a level sufficient for extrusion applications which comprises mechanically working a composition consisting essentially of the copolymer, at a peak temperature below the degradation temperature of the copolymer and for a maximum period of residence time at the peak temperature of 5 minutes.
- Claim 2Depends on #1
The process of claim 1 wherein the copolymer contains at least 35 weight percent vinyl acetate.
- Claim 3Depends on #2
The process of claim 2 wherein the peak temperature is about 40°-225° C.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗