Process for the obtaining of poly(vinylidene fluorine) yarns and fibers
Abstract
A process of making polyvinylidene fluoride yarns and fibers of homogeneous structure and good dry strength includes the steps of spinning the solution of the polymer into a coagulating bath containing 45 to 60% by weight aprotic polar organic solvent and 40 to 55% by weight water, stretching the filaments in air to a ratio of 1.5 to 5x and then in boiling water to a ratio of 1.5 to 4x (overall stretching ratio of 3x to 6.5x) and then washing in water at room temperature.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 4.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A process of making polyvinylidene fluoride yarns and fibers of improved structure and dry tenacity of more than 33 grams/tex, said process comprising: spinning a solution of polyvinylidene fluoride into a coagulating bath containing 45 to 60% by weight aprotic polar organic solvent and 40 to 55% by weight of water maintained between 15° and 40°C, stretching the filaments in air between 15°C and 40°C to a ratio of between 1.5x and 5x, then stretching the filaments in boiling water to a ratio of between 1.5x and 4x, the overall stretch ratio being between 3x and 6.5x, and then washing the fil
- Claim 2Depends on #1
The process as claimed in claim 1, wherein: the aprotic polar organic solvent is dimethylformamide.
- Claim 3Depends on #1
The process as claimed in claim 1, wherein: the apro
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗